Cracks in a brick pier look alarming, but their shape is the first clue to the cause. Here is how to read them, and when to bring in an engineer.
Brick pier cracking happens when the masonry is restrained from moving, or when the ground under it settles unevenly. BIA notes name uneven foundation settlement, moisture growth and temperature change as movement sources, and a tapering crack points to settlement or deflection. These notes were written for walls, so they apply to piers by analogy.
Brick Pier Cracking Starts With the Crack Shape
BIA Technical Notes on Brick Construction 18 says the shape, location and magnitude of cracking will often indicate the cause. Read the crack before you guess at a fix. The notes were written for walls, so this reading applies to piers by analogy.
One pattern stands out. The notes say, “Deflection and settlement cracks are identified by a tapering shape.” A crack that is wide at one end and narrows toward the other fits that pattern.
Foundation Settlement Causes Stepped Cracks
Uneven settlement is a cause BIA names directly for brick. The notes say unstable or expansive soils often cause movement or differential settlement in foundations that support brick masonry. Foundation settlement may then cause diagonal or stepped cracking in the joints directly above the foundation.
For a pier, the mortar joints just above the footing are the place to look. This is an analogy, since the notes address walls. BIA also says proper foundation design helps keep settlement uniform within acceptable limits. For footing depth, read how deep footings should be.
Moisture, Temperature and Bonded Concrete
Brick grows over its service life. BIA says brickwork generally increases in size over time, influenced mainly by irreversible moisture expansion. When that growth is restrained, the masonry can crack.
Temperature changes add to the movement. BIA Technical Note 18A lists temperature change, moisture expansion, elastic deformation, settlement and creep as movements that expansion joints absorb. Failing to allow those movements may result in cracks.
Bonded concrete adds a second restraint. BIA Technical Note 18 says masonry bonded to a cast-in-place concrete slab may crack if the slab curls and lifts the adjacent masonry. Technical Note 18A says bond breaks between foundations and walls let masonry move independently while still resting on its support.
Both notes cover walls and veneer, not free-standing piers. Treat this section as an analogy: a pier tied to a footing or slab faces the same restraint question.
Height, Slenderness and Lean
These notes do not explain lean. Lateral loads from wind, soil pressure or impact were not verified for piers, so this article does not rank them as causes.
The one hard number is the height limit. IRC R606.7, in the South Carolina state copy, says the unsupported height of masonry piers shall not exceed 10 times their least dimension. A pier with a 16-inch least dimension, for example, has a limit of 160 inches (10 x 16).
The 4 times limit applies only to unfilled hollow piers. The state text covers isolated hollow clay tile or hollow concrete masonry piers that support beams and girders. Do not apply it to solid brick. This is the state copy, not the ICC text, which was not read.
Height also sets the course count in the calculator. Bricks are whole units, so every count rounds up. A porch pier with 2 bricks per course, 36 inches tall, 2 piers and 10 percent waste needs 14 courses: 36 / 2.667 = 13.50, rounded up to 14. That gives 2 x 14 x 2 x 1.10 = 61.6, rounded up to 62 bricks.
A gate pier with 4 bricks per course, 48 inches tall, 2 piers and 10 percent waste needs 18 courses: 48 / 2.667 = 17.998, rounded up to 18. Two piers of 4 x 18 give 144 bricks. 144 x 1.10 = 158.4, which rounds up to 159 bricks.
Water, Reinforcement and Loading Points
Water inside the masonry adds risk. BIA recommends minimizing water within masonry through proper design, detailing and installation. It also says to avoid mortar additives that accelerate corrosion, such as calcium chloride.
Technical Note 18A says to use reinforcement at stress concentrations, such as parapets, applied loading points and openings. A pier’s top bearing point is a loading point, so this guidance applies by analogy. Check any reinforcement against the design. For steel cover in concrete footings, see rebar concrete cover.
Load-bearing masonry resists cracking better, according to Technical Note 18A. Compressive stress from dead and live loads helps offset movement. A lightly loaded or free-standing pier has less of that offset, by analogy.
When to Call an Engineer About a Cracked Pier
Work through the crack before you plan a repair. The questions below sort the likely causes. Bring the answers to an engineer or mason.
Call an engineer or mason when any of these holds: the crack is stepped or tapering, the pier leans, the pier carries load or stands free, or the height is near the 10 times limit. The calculator’s disclaimer says a load-bearing or free-standing pier should be confirmed the same way.
Enter the bricks per course, height, pier count and waste in the pier brick and bag estimator to get the count. Then confirm the design with an engineer.
FAQs About Brick Pier Cracks
What most often causes a brick pier to crack?
BIA notes written for walls name uneven foundation settlement as a frequent cause, often tied to unstable soil. No BIA note ranks causes for piers, so treat this as analogy, not a ranking.
Is a tapering crack in a brick pier serious?
A tapering crack matches the settlement or deflection pattern BIA describes. The notes do not rate severity, so have an engineer or mason assess the pier before any repair.
Can moisture alone crack a brick pier?
The notes do not show moisture alone causing cracks. BIA says brickwork grows mainly from moisture expansion, and cracks can form when that growth is restrained.
How tall can a brick pier be?
The South Carolina state copy of IRC R606.7 limits unsupported height to 10 times the least dimension. Isolated unfilled hollow clay tile or hollow concrete masonry piers use a 4 times limit. Check your local code edition.
Does a leaning brick pier mean it will fall?
The notes here do not say. Lean from lateral load was not verified. A leaning pier needs an engineer’s check before you decide it is safe.
Do expansion joints stop brick pier cracks?
BIA says expansion joints prevent cracking by separating masonry into segments. That guidance covers walls and veneer, not free-standing piers, so applying it to a pier is an analogy.
Can I repair a cracked brick pier myself?
Get the crack assessed first. The calculator’s disclaimer says a load-bearing or free-standing pier should be confirmed by an engineer or mason, and its size, bond, reinforcement and footing must follow the design and local code.
Sources and Further Reading
References Used in This Article
- BIA Technical Notes on Brick Construction 18, Volume Changes: Analysis and Effects of Movement, accessed 2026-11-11.
- BIA Technical Notes on Brick Construction 18A, Accommodating Expansion of Brickwork, accessed 2026-11-11.
- South Carolina Code of Regulations 8-1226, IRC R606.7 Piers (state-adopted copy), accessed 2026-11-11.
Cause statements come from BIA notes written for walls, applied to piers by analogy. Have an engineer check a cracked pier before repair. Reviewed for accuracy by Prof. Dr. Khalil Mudassar, PhD. Last updated 2026-11-11.

Shakeel Muzaffar is the Founder and Editor-in-Chief, with over 15 years of experience in digital publishing and online tool development. He oversees editorial quality and formula verification to ensure accurate, practical, and easy-to-use calculators.